Processing and properties of magnesium containing a dense uniform dispersion of nanoparticles
LY Chen, JQ Xu, H Choi, M Pozuelo, X Ma, S Bhowmick, JM Yang, ...
Nature 528 (7583), 539-543, 2015
6602015
A sinusoidally-architected helicoidal biocomposite
NA Yaraghi, N Guarín-Zapata, LK Grunenfelder, E Hintsala, S Bhowmick, ...
arXiv preprint arXiv:1604.07798, 2016
1922016
Atomically thin gallium layers from solid-melt exfoliation
V Kochat, A Samanta, Y Zhang, S Bhowmick, P Manimunda, SAS Asif, ...
Science advances 4 (3), e1701373, 2018
1742018
Powder metallurgical processing of equiatomic AlCoCrFeNi high entropy alloy: Microstructure and mechanical properties
S Mohanty, TN Maity, S Mukhopadhyay, S Sarkar, NP Gurao, S Bhowmick, ...
Materials Science and Engineering: A 679, 299-313, 2017
1642017
A natural impact-resistant bicontinuous composite nanoparticle coating
W Huang, M Shishehbor, N Guarín-Zapata, ND Kirchhofer, J Li, L Cruz, ...
Nature Materials 19 (11), 1236-1243, 2020
1292020
Failure modes in ceramic‐based layer structures: a basis for materials design of dental crowns
B Lawn, S Bhowmick, MB Bush, T Qasim, ED Rekow, Y Zhang
Journal of the American Ceramic Society 90 (6), 1671-1683, 2007
1132007
Competition of fracture mechanisms in monolithic dental ceramics: flat model systems
Y Zhang, JW Kim, S Bhowmick, VP Thompson, ED Rekow
Journal of Biomedical Materials Research Part B: Applied Biomaterials: An …, 2009
1032009
Contact damage in TiN coatings on steel
S Bhowmick, AN Kale, V Jayaram, SK Biswas
Thin Solid Films 436 (2), 250-258, 2003
882003
Transverse fracture of brittle bilayers: relevance to failure of all‐ceramic dental crowns
JW Kim, S Bhowmick, I Hermann, BR Lawn
Journal of Biomedical Materials Research Part B: Applied Biomaterials: An …, 2006
802006
Piezoresistive response of quasi-one-dimensional ZnO nanowires using an in situ electromechanical device
S Kaps, S Bhowmick, J Grottrup, V Hrkac, D Stauffer, H Guo, OL Warren, ...
Acs Omega 2 (6), 2985-2993, 2017
752017
3D porous graphene by low-temperature plasma welding for bone implants
D Chakravarty, CS Tiwary, CF Woellner, S Radhakrishnan, S Vinod, ...
Adv. Mater 28 (40), 8959-8967, 2016
642016
Competing fracture modes in brittle materials subject to concentrated cyclic loading in liquid environments: Trilayer structures
I Hermann, S Bhowmick, Y Zhang, BR Lawn
Journal of materials research 21 (2), 512-521, 2006
572006
Contact deformation of TiN coatings on metallic substrates
V Jayaram, S Bhowmick, ZH Xie, S Math, M Hoffman, SK Biswas
Materials Science and Engineering: A 423 (1-2), 8-13, 2006
562006
Competing fracture modes in brittle materials subject to concentrated cyclic loading in liquid environments: Monoliths
Y Zhang, S Bhowmick, BR Lawn
Journal of Materials Research 20 (8), 2021-2029, 2005
532005
Deconvolution of fracture properties of TiN films on steels from nanoindentation load–displacement curves
S Bhowmick, V Jayaram, SK Biswas
Acta materialia 53 (8), 2459-2467, 2005
522005
Competing fracture modes in brittle materials subject to concentrated cyclic loading in liquid environments: Bilayer structures
S Bhowmick, Y Zhang, BR Lawn
Journal of Materials Research 20 (10), 2792-2800, 2005
502005
Nature of contact deformation of TiN films on steel
S Bhowmick, ZH Xie, M Hoffman, V Jayaram, SK Biswas
Journal of materials research 19, 2616-2624, 2004
452004
Role of indenter material and size in veneer failure of brittle layer structures
S Bhowmick, JJ Meléndez‐Martínez, I Hermann, Y Zhang, BR Lawn
Journal of Biomedical Materials Research Part B: Applied Biomaterials 82 (1 …, 2007
412007
Magnetic field controlled graphene oxide-based origami with enhanced surface area and mechanical properties
OK Park, CS Tiwary, Y Yang, S Bhowmick, S Vinod, Q Zhang, VL Colvin, ...
Nanoscale 9 (21), 6991-6997, 2017
402017
Temperature dependent fracture initiation in microscale silicon
ED Hintsala, S Bhowmick, X Yueyue, R Ballarini, SAS Asif, WW Gerberich
Scripta Materialia 130, 78-82, 2017